Emballage de bobine avec boîte en carton, emballage de bobine avec poly-sac, emballage de caisse en
Capacité d'approvisionnement:
1200 tonnes par mois
Mettre en évidence:
GH3044 superalloy wire 0.5-6.0mm
,
high temp nickel alloy wire
,
superalloy wire for fasteners
Description du produit
Solid-solution strengthened GH3044 nickel-chromium superalloy wire engineered for critical high-temperature fasteners, aerospace structural components, and high-heat springs. Manufactured through high-purity vacuum metallurgy and multi-pass precision drawing for superior thermal stability and fatigue strength. Product Overview The high-temperature fastening sector demands raw materials with flawless surface quality, uniform chemical distribution, and consistent mechanical